Inner Conductor: Cu 0,8mm
Physical expansion dielectric triple layer Φ(+/-0,1): PEG 3,5
Screening tape: Al 3+
Screening percentage: 100%
Screen: Al
Screening percentage: 75%
Jacket (+/- 0,2): PVC 5mm
Minimum bending radius OUT/IN mm: 40/20
Nomimal Impedance (Ohm+/-3): 75
Capacitance (pF/m=/-2): 52
Velocity ratio: 85%
Attenuation at 20°C:
- MHz 5 (dB/100m):1,3
- MHz 50 (dB/100m):5,5
- MHz 200 (dB/100m): 10,6
- MHz 470 (dB/100m):16,9
- MHz 860 (dB/100m):23,6
- MHz 1000 (dB/100m):25,6
- MHz 1750 (dB/100m):34,4
- MHz 2050 (dB/100m):37,5
- MHz 2150 (dB/100m):38,2
- MHz 2400 (dB/100m):40,5
- MHz 3000 (dB/100m):45,4
Structure Return Loss (SRL) at:
- 30-300 MHz dB:>33
- 300-600 MHz dB:>30
- 600-9000 MHz dB:>27
Screening efficiency:
- 100-300 MHz dB: >90
- 300-600 MHz dB: >90
- 600-900 MHz dB: >90
Inner Conductor resistance Ohm/Km: 35
Outer Conductor resistance Ohm/Km: 36,6
Tension test of the jacket: 4kV